TY - JOUR
T1 - Experimental assessment for the photon shielding features of silicone rubber reinforced by tellurium borate oxides
AU - Elsafi, M.
AU - Alasali, Heba Jamal
AU - Almuqrin, Aljawhara H.
AU - Mahmoud, K. G.
AU - Sayyed, M. I.
N1 - The authors express their gratitude to the Princess Nourah bint Abdulrahman University Researchers Supporting Project number (PNURSP2023R2), Princess Nourah bint Abdulrahman University, Riyadh, Saudi Arabia.
PY - 2023
Y1 - 2023
N2 - In the present study, six silicone rubber doped by tellurium borate oxides were fabricated using the casting method. The densities of the fabricated silicon rubber-doped by tellurium borate oxides samples were measured using the Archimedes Method. Moreover, the linear attenuation coefficient of silicone rubber doped tellurium borate oxides samples was evaluated experimentally using the hyper pure germanium, and the recorded linear attenuation coefficient values were affirmed using the theoretical Phy-X program. The experimental measurements were performed using the narrow beam transmission method with radioactive isotopes Am-241, Cs-137, and Co-60 with energies of 59, 661, 1173, and 1332 keV. The linear attenuation coefficient values showed an enhancement by 4.73 times, 1.20 time, 1.17, time, and 1.17 time, respectively at gamma photon energies of 59, 661, 1173, and 1332 keV, when the TeO2 concentration increased in the fabricated composites from 0 to 50 wt%. The enhancement of the linear attenuation coefficient values has a positive effect on the transmission rate values where the half-value thickness and transmission rate were decreased accompanied by an increase in the RPE. © 2023 Korean Nuclear Society.
AB - In the present study, six silicone rubber doped by tellurium borate oxides were fabricated using the casting method. The densities of the fabricated silicon rubber-doped by tellurium borate oxides samples were measured using the Archimedes Method. Moreover, the linear attenuation coefficient of silicone rubber doped tellurium borate oxides samples was evaluated experimentally using the hyper pure germanium, and the recorded linear attenuation coefficient values were affirmed using the theoretical Phy-X program. The experimental measurements were performed using the narrow beam transmission method with radioactive isotopes Am-241, Cs-137, and Co-60 with energies of 59, 661, 1173, and 1332 keV. The linear attenuation coefficient values showed an enhancement by 4.73 times, 1.20 time, 1.17, time, and 1.17 time, respectively at gamma photon energies of 59, 661, 1173, and 1332 keV, when the TeO2 concentration increased in the fabricated composites from 0 to 50 wt%. The enhancement of the linear attenuation coefficient values has a positive effect on the transmission rate values where the half-value thickness and transmission rate were decreased accompanied by an increase in the RPE. © 2023 Korean Nuclear Society.
UR - http://www.scopus.com/inward/record.url?partnerID=8YFLogxK&scp=85159192144
UR - https://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcAuth=tsmetrics&SrcApp=tsm_test&DestApp=WOS_CPL&DestLinkType=FullRecord&KeyUT=001003019300001
U2 - 10.1016/j.net.2023.02.022
DO - 10.1016/j.net.2023.02.022
M3 - Article
VL - 55
SP - 2166
EP - 2171
JO - Nuclear Engineering and Technology
JF - Nuclear Engineering and Technology
SN - 1738-5733
IS - 6
ER -
ID: 39238889