  • M. Elsafi
  • Heba Jamal Alasali
  • Aljawhara H. Almuqrin
  • K. G. Mahmoud
  • M. I. Sayyed
In the present study, six silicone rubber doped by tellurium borate oxides were fabricated using the casting method. The densities of the fabricated silicon rubber-doped by tellurium borate oxides samples were measured using the Archimedes Method. Moreover, the linear attenuation coefficient of silicone rubber doped tellurium borate oxides samples was evaluated experimentally using the hyper pure germanium, and the recorded linear attenuation coefficient values were affirmed using the theoretical Phy-X program. The experimental measurements were performed using the narrow beam transmission method with radioactive isotopes Am-241, Cs-137, and Co-60 with energies of 59, 661, 1173, and 1332 keV. The linear attenuation coefficient values showed an enhancement by 4.73 times, 1.20 time, 1.17, time, and 1.17 time, respectively at gamma photon energies of 59, 661, 1173, and 1332 keV, when the TeO2 concentration increased in the fabricated composites from 0 to 50 wt%. The enhancement of the linear attenuation coefficient values has a positive effect on the transmission rate values where the half-value thickness and transmission rate were decreased accompanied by an increase in the RPE. © 2023 Korean Nuclear Society.
Язык оригиналаАнглийский
Страницы (с-по)2166-2171
Число страниц6
ЖурналNuclear Engineering and Technology
Том55
Номер выпуска6
DOI
СостояниеОпубликовано - 2023

    Предметные области WoS

  • Ядерные науки и технологии

    Предметные области ASJC Scopus

  • Nuclear Energy and Engineering

ID: 39238889