Standard

BRANN forecast of superalloy tensile strength versus Larson–Miller parameter relation and its approximation by a sigmoidal function. / Tarasov, Dmitry; Tyagunov, Andrey; Milder, Oleg.
в: Mathematical Methods in the Applied Sciences, Том 46, № 16, 15.11.2023, стр. 16401-16414.

Результаты исследований: Вклад в журналМатериалы конференцииРецензирование

Harvard

APA

Vancouver

Tarasov D, Tyagunov A, Milder O. BRANN forecast of superalloy tensile strength versus Larson–Miller parameter relation and its approximation by a sigmoidal function. Mathematical Methods in the Applied Sciences. 2023 нояб. 15;46(16):16401-16414. doi: 10.1002/mma.8952, 10.1002/mma.v46.16

Author

BibTeX

@article{ae227956c75145a4b6677b3a50f95733,
title = "BRANN forecast of superalloy tensile strength versus Larson–Miller parameter relation and its approximation by a sigmoidal function",
abstract = "Nickel-based superalloys are unique materials with complex doping that demonstrate excellent resistance to mechanical and chemical degradation. Over a long period of use in industry, a variety of information has been accumulated about their possible chemical compounds and features corresponding to a certain composition. One of the main service properties of the alloy is the tensile strength (σ). For a more convenient comparison of the characteristics of the alloys with different chemical compositions, the temperature and holding time of the metal during testing are often combined into a complex Larson–Miller parameter (PLM). The availability of experimental or simulated data on the alloys' properties in the entire range of temperatures and exposures would significantly expand the possibilities of the alloy applications and would allow a more accurate evaluation and comparison of the alloys. In this work, we use a machine learning method for modeling the properties of the alloys according to their composition. A Bayesian regularized artificial neural network was engaged to simulate missing tensile strength values for 278 superalloys. Special data preprocessing and the use of an ensemble of networks during training reduced the model error. Comparison of the predicted and experimental data showed excellent convergence. The method made it possible to obtain enough data to approximate the relation (Figure presented.) with a sigmoid function. The slope coefficient is considered as a quantitative expression of the thermal stability of the superalloys.",
author = "Dmitry Tarasov and Andrey Tyagunov and Oleg Milder",
year = "2023",
month = nov,
day = "15",
doi = "10.1002/mma.8952",
language = "English",
volume = "46",
pages = "16401--16414",
journal = "Mathematical Methods in the Applied Sciences",
issn = "0170-4214",
publisher = "John Wiley & Sons Inc.",
number = "16",

}

RIS

TY - JOUR

T1 - BRANN forecast of superalloy tensile strength versus Larson–Miller parameter relation and its approximation by a sigmoidal function

AU - Tarasov, Dmitry

AU - Tyagunov, Andrey

AU - Milder, Oleg

PY - 2023/11/15

Y1 - 2023/11/15

N2 - Nickel-based superalloys are unique materials with complex doping that demonstrate excellent resistance to mechanical and chemical degradation. Over a long period of use in industry, a variety of information has been accumulated about their possible chemical compounds and features corresponding to a certain composition. One of the main service properties of the alloy is the tensile strength (σ). For a more convenient comparison of the characteristics of the alloys with different chemical compositions, the temperature and holding time of the metal during testing are often combined into a complex Larson–Miller parameter (PLM). The availability of experimental or simulated data on the alloys' properties in the entire range of temperatures and exposures would significantly expand the possibilities of the alloy applications and would allow a more accurate evaluation and comparison of the alloys. In this work, we use a machine learning method for modeling the properties of the alloys according to their composition. A Bayesian regularized artificial neural network was engaged to simulate missing tensile strength values for 278 superalloys. Special data preprocessing and the use of an ensemble of networks during training reduced the model error. Comparison of the predicted and experimental data showed excellent convergence. The method made it possible to obtain enough data to approximate the relation (Figure presented.) with a sigmoid function. The slope coefficient is considered as a quantitative expression of the thermal stability of the superalloys.

AB - Nickel-based superalloys are unique materials with complex doping that demonstrate excellent resistance to mechanical and chemical degradation. Over a long period of use in industry, a variety of information has been accumulated about their possible chemical compounds and features corresponding to a certain composition. One of the main service properties of the alloy is the tensile strength (σ). For a more convenient comparison of the characteristics of the alloys with different chemical compositions, the temperature and holding time of the metal during testing are often combined into a complex Larson–Miller parameter (PLM). The availability of experimental or simulated data on the alloys' properties in the entire range of temperatures and exposures would significantly expand the possibilities of the alloy applications and would allow a more accurate evaluation and comparison of the alloys. In this work, we use a machine learning method for modeling the properties of the alloys according to their composition. A Bayesian regularized artificial neural network was engaged to simulate missing tensile strength values for 278 superalloys. Special data preprocessing and the use of an ensemble of networks during training reduced the model error. Comparison of the predicted and experimental data showed excellent convergence. The method made it possible to obtain enough data to approximate the relation (Figure presented.) with a sigmoid function. The slope coefficient is considered as a quantitative expression of the thermal stability of the superalloys.

UR - http://www.scopus.com/inward/record.url?partnerID=8YFLogxK&scp=85144265962

UR - https://gateway.webofknowledge.com/gateway/Gateway.cgi?GWVersion=2&SrcAuth=tsmetrics&SrcApp=tsm_test&DestApp=WOS_CPL&DestLinkType=FullRecord&KeyUT=000898792900001

U2 - 10.1002/mma.8952

DO - 10.1002/mma.8952

M3 - Conference article

VL - 46

SP - 16401

EP - 16414

JO - Mathematical Methods in the Applied Sciences

JF - Mathematical Methods in the Applied Sciences

SN - 0170-4214

IS - 16

ER -

ID: 47866061