The phase composition and the morphology of structures formed as a result of isothermal holds in the range of aging temperatures of hardened alloy Fe - 28% Mn, 8.5% Al - 1% C - 1.25% S arc studied. A diagram of the decomposition of initial austenite is plotted starting with the early stages and ending with the moment when the system attains the equilibrium state.