Samples of the buildup in a mixer processing low-silica vanadium hot metal undergo chemical and X-ray microspectral analysis. The buildup consists of high-temperature spinelide, ilmenite, magnetite, and other phases. The mechanism by which the buildup forms is established, and measures for its prevention are developed.