Fe-Cr-C-T-Al flux-cored wire surfacing was performed by laser, arc and hybrid methods. Laboratory tests have shown that the deposited layers vary greatly in terms of wear resistance. To identify the reasons, studies were carried out using metallographic, X-ray structural and durometric methods. The analysis of the research results showed that the reason is the difference in the cooling rates of the deposited metal in the range of 1100-800 K. This difference leads to the possibility of the formation of a metastable austenitic structure, which, in turn, affects the wear resistance of the deposited layers.
Translated title of the contributionPECULIARITIES OF TRANSFORMATION OF METASTABLE AUSTENITE INTO DEFORMATION MARTENSITE DURING LASER CLADDING WITH CORED WIRE 60CR7TIAL
Original languageRussian
Pages (from-to)1967-1973
Number of pages7
JournalФизика твердого тела
Volume63
Issue number12
DOIs
Publication statusPublished - 2021

    GRNTI

  • 29.00.00 PHYSICS

    Level of Research Output

  • VAK List
  • Russian Science Citation Index

ID: 23831087